Magnesium Anode

﹛﹛Chemical Composition of Mg Sacrificed Anode(%)
Elements
Mg anode with high electric potential
AZ63B
AZ63C
AD63D
Al <0.01 5.30-6.70 5.30-6.70 5.0-7.0
Zn ... 2.50-3.50 2.50-3.50 2.0-4.0
Mn 0.50-1.30 0.15-0.70 0.15-0.70 0.15-0.70
Si(max) 0.05 0.10 0.30 0.30
Cu(max) 0.02 0.02 0.05 0.10
Ni(max) 0.001 0.002 0.003 0.003
Fe(max) 0.03 0.003 0.003 0.003
Other metal impurity(max) 0.05 --- --- ---
Total of impurities(max) 0.30 0.30 0.30 0.30
Mg Remains Remains Remains Remains

﹛﹛Electrochemical properties of Mg sacrificed anodes

Tel: 86-311-87030619 / 87015576 Fax: 86-311-87033670 ﹛E-mail: hemtec@163.net ﹛Head office: 3 North Zhonghua Street, Shijiazhuang City, Hebei, P.R. China﹛﹛P.C.: 050000

Product\Item
Open-circuit voltage(-V)
Closed-circuit voltage(-V)
Actual Capacitance(A.h/g)
Current efficiency(%)
Mg anode with high electric potential 1.70~1.75 1.57~1.62 1.100 min. 50 min.
AZ63Mg anode 1.50~1.55 1.45~1.50 1.105 min. 50 min.